How many points does a patterned plate need before you can call it uniform?
A sampling plan is a probability statement, not a coverage guarantee. Twenty-five points give a usable uniformity number and a 4.8 % chance of finding a 10 mm fault.
By TL OPTIK
The short answer
Two different questions arrive with the word sampling. "How uniform is this plate?" is a continuous quantity: it can be estimated from a few well-placed points, and the estimate gets better as you add more. "Is there a bad zone on it?" is a discrete event: it cannot be estimated at all, because a fault either falls under a measured point or it does not.
Twenty-five points on a 200 mm plate are a defensible uniformity sample and a poor fault detector; nothing about the number of points fixes that. What fixes it is writing down which job the plan is doing, and then sizing it for that job. A plan that does not name its job cannot be quoted against, cannot be repeated by a second lab, and cannot settle a disagreement between the two.
The two jobs a sampling plan can do
TL OPTIK's own pages already treat sampling as a required input without sizing it. The laser direct writing page lists what the final mask depends on and names inspection sampling in that list. The measuring microscope page puts measurement locations and sampling plan among the items to define before measuring. The quality page says sampling is confirmed per project, and draws a line that matters here: keep dimensional results separate from defect classification. That line is the whole argument of this guide, so it is worth taking literally.
A dimensional result is a number on a continuous scale. Two plates with the same mean line width and different spreads are different plates, and a sample of the spread is meaningful. A defect is not a number on that scale: it is present or absent at a location, and no amount of averaging turns an unsampled location into an inspected one. Three separate purposes follow, and they need three different plans.
| Purpose | The question it answers | What the data must contain | Points for a usable answer | What it cannot tell you |
|---|---|---|---|---|
| Estimate the field | How uniform is the pattern across this plate? | A mean and a spread, with the point count and the statistic named | 25–50 | Anything about a fault 10 mm across |
| Verify one feature | Is this measured line inside the window? | One value at a named coordinate under a named method | 1 per feature | The rest of the plate |
| Find a local fault | Is there a bad zone anywhere on this plate? | Coverage, and a stated probability of detection | 1,172 for 90 % | Anything that falls between the points |
Point counts are arithmetic on the 200 mm plate used throughout this page; they are not recommendations for any particular order. The two right-hand columns are the reason a drawing should say which purpose it means.
What one measurement point actually covers
Before the statistics, the geometry, because the geometry is what people overestimate. A measurement point is not a reading of the plate. It is a reading of the field the instrument resolves at that coordinate — a patch of a fraction of a millimetre, set by magnification and by how much of the image the operator measures.
Take a 200 mm square plate, forty thousand square millimetres, and a 0.1 mm field per point. Twenty-five points then cover 0.25 mm². One part in 160,000 of the plate.
This is not an argument against sampling. It is an argument about what a sample can be asked to prove. Twenty-five readings placed with care will tell you the centre and the spread of a continuous field well enough to compare a plate with a 55 nm limit, in the way a handful of thermometers tells you the temperature of a room. They will not tell you whether a 10 mm zone in the corner is bad, any more than those thermometers tell you whether a window is open.
Why the coverage number is so small
The fraction is tiny because the plate is large compared with the instrument's field, not because the plan is careless. A 200 mm plate is 200,000 µm on a side; a 0.1 mm field is 100 µm on a side. Each point therefore reads one part in two thousand of one edge length. Multiply by 25 points and the covered area is still a rounding error against the plate.
Two consequences follow directly. First, a plan can only be judged against the size of the thing it is supposed to find. Second, the only way to change the coverage is to change what is measured — a wider field, a scan, or a different instrument — not to add points. Adding points improves an estimate; it barely moves coverage.
How many points before a uniformity number means something
A uniformity figure is a standard deviation, usually quoted at 3σ. The published writer reference gives 55, 65 and 75 nm at 3σ for three writing configurations. Those are equipment values for route selection, not promises about a delivered part, and they carry a property that is rarely written down: a standard deviation estimated from n points is itself uncertain, and the uncertainty depends only on how many points were used.
The arithmetic is the χ² interval on a variance estimate with n − 1 degrees of freedom. With nine points a reported 55 nm 3σ is consistent, at 90 % confidence, with a true spread anywhere from 39.5 nm to 94.1 nm. With 25 points the bracket narrows to 44.7–72.4 nm; with 49 points to 47.2–66.2 nm; with 100 points to 49.3–62.3 nm.
Read that the other way round and it becomes a purchasing question. If a drawing says 55 nm and a report from nine points returns 52 nm, the report has not demonstrated conformity; the bracket still contains 94 nm. If the same drawing is checked with 49 points and returns 52 nm, the bracket is 45–63 nm and the pass is defensible. The number of points is part of the requirement, not an implementation detail left to whoever inspects.
Which numbers are which. The 55 / 65 / 75 nm CD uniformity, 30 / 40 / 50 nm edge roughness and 12.5 / 25 nm address grid are published equipment reference values for the three direct-write configurations, used to choose a writing route. They are not a product guarantee and not a measurement uncertainty. Every interval on this page is arithmetic on those values; the point counts and the 90 % confidence level are inputs chosen for illustration.
Industry reference only. This does not represent a confirmed TL OPTIK capability or a guaranteed supplier specification. Final requirements must be reviewed and agreed in writing.
Points per writing field, not points per area
There is a second constraint that area coverage hides. A written plate is not one continuous field: the writer covers it in fields of 205 × 205 mm or 410 × 410 mm, and where two fields meet there is a stitching boundary with its own published stability, 30 to 70 nm at 3σ depending on configuration. A field boundary produces a step, and a plan with no points near the boundary will not see it.
Two points per writing field is the minimum that can separate a field-to-field step from scatter inside a field, because a step is a difference between groups and a difference needs at least two members per group. On a 228.6 mm plate that means eight points before the plan can say anything about stitching at all — which is a floor, not an answer, since eight points say nothing useful about the spread.
| Format | Side, mm | Area, mm² | 10 mm band | Writing fields | Of 25 points, in the band |
|---|---|---|---|---|---|
| 3 in | 76.2 | 5,806 | 45.6 % | 1 | 11 |
| 4 in | 101.6 | 10,323 | 35.5 % | 1 | 9 |
| 6 in | 152.4 | 23,226 | 24.5 % | 1 | 6 |
| 9 in | 228.6 | 52,258 | 16.7 % | 4 | 4 |
| 17 in | 431.8 | 186,451 | 9.0 % | 4 | 2 |
Formats from the published 3–9 in substrate class and the 9 × 9 / 17 × 17 in writer formats; band share and point counts are arithmetic on a 10 mm excluded border. Field counts assume a 2 × 2 layout when the side exceeds the published 205 mm or 410 mm field. A 17 in plate can also be written as a single 410 mm field with the remaining 21.8 mm left as margin, which is a drawing decision rather than a sampling one.
How many points to find a defect
The defect question has an exact answer, and it is uncomfortable. If f is the area of the fault divided by the area of the plate, and n points are placed independently, the probability that at least one point lands inside the fault is P = 1 − (1 − f)ⁿ.
A 10 mm fault is 78.5 mm² on a 40,000 mm² plate, one part in 509. Put 25 points at random and the chance that one of them lands inside is 4.8 %. To reach 90 % you need 1,172 points — on a part whose useful inspection time is minutes. For a 5 mm fault the same 90 % needs 4,690 points, so the answer to "how many points do I need to find a defect" is not a number of points at all.
That is not a failure of sampling; it is the wrong tool for the task. A defect on a patterned plate is found by covering the area — an automatic optical inspection pass over the active field, an operator scan at defined magnification over the zones that matter, or an agreed rule about how much area is inspected at what sensitivity. Sampling enters afterwards, as a check on the inspection, not as a replacement for it.
Counting points does help
- Estimating the spread of a continuous quantity
- Comparing a plate with a stated limit
- Detecting a large-scale gradient across the plate
- Detecting a field-to-field step, at two points per field
Counting points does not help
- Finding a local fault of unknown position
- Proving the absence of a defect anywhere
- Replacing an area scan over the functional zones
- Confirming a defect limit nobody wrote down
Where the points go
If the points are going to be few, their position carries most of the information the plan will ever have. Three placements on the same plate give three different answers, and only one of them is a default.
The first plan puts every point 20 mm or more from the edge. That is exactly what a grid drawn on a drawing looks like, and it means the outer band — 19 % of a 200 mm plate, 45.6 % of a 3 in plate — is not sampled at all. If the process tends to fail near the cut edge, which is the case whenever chip, bevel and edge exclusion are involved, that band is where the interesting variation lives.
The second plan moves five of the 25 points into the band, roughly in proportion to its area, and adds nothing else. It is the cheapest improvement available: same instrument, same time, a different drawing.
The third plan places points where the part does work — inside the pattern, plus the four alignment marks. It samples almost none of the plain border, which is usually correct, and it is the plan that matches how the part will actually fail in service. It is also the plan that is hardest to write generically, because it needs the zone map.
None of the three is wrong. The mistake is to draw the first one, call it uniformity, and then be surprised by a fault in a band that no point could reach. The zone map decides the plan; the plan does not decide the zone map. TL OPTIK's inspection guide already asks for the zones to be defined before the limits; this page is about what to do once they are.
Three statistics from one data set
The last thing a plan has to name is the number it reports, because the same readings support three different verdicts. Take nine site readings from one plate, expressed as deviations from the nominal line width, and a limit of ±25 nm applied to the part.
| Statistic | Value | Against ±25 nm | What it says |
|---|---|---|---|
| Mean of the nine sites | +13.0 nm | Pass | On average the plate is inside the window |
| 3σ of the same nine | 33.1 nm | Fail | Read as a limit, the spread is outside the window |
| Largest single reading | +34 nm | Fail | One site is outside; the part is rejected |
The nine readings are a constructed example chosen to separate the three statistics; they are not measurements of any part, and 33.1 nm is 3 × 11.03 nm. A drawing that says "line width" and a report that gives a maximum will disagree at any sample size without anyone making a mistake.
All three numbers come from one set of readings and all three are computed correctly. Which one the limit applies to is a contract term, and it belongs next to the tolerance in the same sentence. There is a second, quieter version of the same problem on the measurement side: a reported spread contains the repeatability of the instrument as well as the plate, so a conforming plate can report slightly worse than it is. That term, and how large it is for a chrome edge, is the subject of why two labs measure a different line width; the point here is only that the statistic has to be named before the values are compared.
Write the plan into the drawing and the RFQ
A sampling plan that lives in an email thread is not reproducible. Six fields put it in the documents, and the fifth is the one that saves the argument.
| Field | What to write | Why it changes the answer |
|---|---|---|
| Zone map | Functional area, clear aperture, alignment marks, excluded border, each dimensioned on the DWG | A limit without a zone cannot be applied to a point |
| Points and coordinates | The count, and the coordinate of each point referenced to the drawing datum | Makes a second lab repeat the check at the same place |
| Statistic | Mean and 3σ, or maximum deviation, or all points within — named explicitly | Three valid numbers come from one data set |
| Decision rule | How a value inside the measurement uncertainty is treated against the limit | Stops a borderline part being rounded into compliance |
| Coverage statement | What this plan does not cover: faults below a stated size, areas outside the zone map | Turns an assumption into a sentence both parties signed |
| Report content | Drawing revision, coordinates, method, values, units, judgement, images | The customer can re-check without another conversation |
These are drafting prompts for a discussion, not a description of any TL OPTIK default. The inspection scope, sampling and documents for an order are confirmed with the order, and a delivered part is judged against its approved drawing and inspection plan.
Two of these fields are usually absent from the first draft of an order, and they are the two that cause the most correspondence later: the coordinates, and the coverage statement. The coordinates are cheap to give and they end the "we measured it and it was fine" exchange immediately. The coverage statement is harder, because it requires saying out loud that 25 points do not cover a plate — which is exactly the sentence that prevents the dispute.
What this guide does not establish
- It does not state a default sampling plan for TL OPTIK, and there is no published point count for any product. Sampling is confirmed per order, together with the inspection scope.
- It does not give a measurement uncertainty for any instrument, a minimum detectable defect size, or an acceptance threshold for defects.
- It does not claim that the 55 / 65 / 75 nm CD uniformity values describe a delivered part. They are equipment reference values for three writing configurations, published for route selection.
- It does not treat the 0.1 mm field, the 25-point plans, the 10 mm band or the ±25 nm limit as product values. They are inputs chosen to make the arithmetic visible, and each one changes the numbers on this page.
- It says nothing about price, lead time, minimum order quantity or yield, none of which is published.
Questions that come up before an order
Is 25 points enough to call a plate uniform?
For a plate-wide standard deviation, 25 points put the estimate within roughly ±20 % at 90 % confidence, which is usually enough to compare a part with a limit and to notice a change between two runs. For finding a local fault it is not enough at all: on a 200 mm plate, 25 points have about a 4.8 % chance of landing inside a 10 mm fault. Both statements are true of the same plan, which is why the plan has to say which job it is doing.
Should the points be on a grid or placed at random?
A grid is reproducible: a second lab can return to the same coordinates and the two results can be compared point by point. Random placement is unbiased for detection, but it cannot be repeated, so a disagreement becomes unarguable. Use a grid, then add the points a grid can structurally miss. A writing-field boundary is the clearest case: on a 431.8 mm plate written as two 410 mm fields with the boundary at 410 mm from the reference edge, a two-column grid samples 108 mm and 324 mm and comes no closer than 86 mm to the seam. The seam itself has to be sampled deliberately.
How many points should a 3 inch plate have?
The question is misleading on a small format. On a 76.2 mm plate a 10 mm edge band is 45.6 % of the area, so an interior grid describes less than half the part, and the "uniformity over the plate" that a drawing asks for is dominated by a border that a conventional plan skips. Place points by zone instead: the band, the functional pattern, and the marks. The count matters less than the fact that all three appear on the plan.
Is a note saying "55 nm 3σ CD uniformity" a complete requirement?
No. It names a limit without naming the point count, the zone, the statistic, the measurement method or the decision rule, and each of those can change the verdict on a conforming part. Read from nine points, a 55 nm 3σ figure is consistent with a real spread anywhere between about 40 nm and 94 nm at 90 % confidence. Adding the point count to the sentence costs nothing and removes most of that ambiguity.
Can I compare two suppliers' uniformity numbers?
Only when the point count, the zone, the statistic, the edge-definition method and the writing configuration are the same. Otherwise a lower number may mean a better plate, or merely fewer points, a different statistic, or a measurement made over a friendlier area. The comparison is worth making only after both reports name their plan. Two reports that do are directly comparable; two that do not are two anecdotes.
Can sampling replace a full inspection of the plate?
For a continuous quantity such as line width, a sample estimates the field and that is a legitimate basis for acceptance. For a discrete defect, sampling gives a probability of detection and never a guarantee, whatever the point count. Defect acceptance therefore needs either full-area inspection of the defined zones or an agreed statistical plan with a stated confidence and a stated zone. If neither is written down, the acceptance criterion is not "no defects"; it is "no defects that this plan happened to see".
Send the zone map, the limit and the plan
Chrome patterns on glass, fused silica and ceramic are quoted from an approved drawing with a stated inspection method. If the sampling plan is the open question, say so in the enquiry: it is easier to agree before the plate is written than after two labs have measured it differently.
Where each figure comes from
The published values below are the only numbers this page takes as given. Everything else — the 200 mm plate, the 0.1 mm field, the 25-point plans, the 10 mm band, the ±25 nm limit and the point-count arithmetic — is derived from them and stated as arithmetic where it appears.
| Figure used here | Where it is published |
|---|---|
| CD uniformity 55 / 65 / 75 nm at 3σ; edge roughness 30 / 40 / 50 nm at 3σ; address grid 12.5 / 25 nm; minimum feature 0.75 / 1 µm; stitching stability 30 / 60 / 70 nm | Laser direct writing — three configuration reference table |
| Writing fields 205 × 205 mm and 410 × 410 mm; formats 9 × 9 in and 17 × 17 in; substrate thickness 0–12 mm; "the final mask still depends on … inspection sampling" | Laser direct writing — capacity and dependencies |
| Substrate class 3–9 in; thickness ≥0.3 mm; TTV ≤2 µm; flatness ≤2 µm; the two flatness schedules | Chrome-coated photomask blanks: flatness and defect grades |
| ±0.2 µm line-width reference, with acceptance qualified as "according to approved drawing, inspection area and measurement method" | Why two labs measure a different line width and chrome-on-glass photomasks |
| "Measurement locations and sampling plan" as an input to be defined before measuring | Precision measuring microscope |
| Sampling confirmed per order; "keep dimensional results separate from defect classification" | Quality, inspection and delivery |
| The zone-before-limit order of questions, and the decision rule at a tolerance limit | Inspection and acceptance of patterned glass |